GMAW (Spray Transfer) ER70S-6 90%Ar / 10% Co2
$150.00
AWS D1.1 Prequalified WPS (PWPS) GMAW SprayTransfer ER70S-6 Plate 90% Ar / 10% Co2
- AWS D1.1: 2015 Prequalified Welding Procedure Specification (WPS)
- Qualifies the following:
- Common prequalified groove and fillet joints
- Flat position
- D1.1 Group I to Group I, Group II to Group I, and Group II to Group II
- 1/8 in. to 3/4 in. base metal thickness