AWS D1.1 Prequalified WPS (PWPS) SMAW, All Position, E7018 Welding
$150.00
AWS D1.1 Prequalified WPS (PWPS) SMAW, All Position, E7018 Welding
- AWS D1.1: 2015 Prequalified Welding Procedure Specification (WPS)
- Qualifies the following:
- Common prequalified groove and fillet joints (note - open root joints are not prequalified)
- Flat, Vertical, Horizontal and Overhead positions
- D1.1 Group I to Group I, Group II to Group I, and Group II to Group II
- 1/8 in. to 3/4 in. base metal thickness or up to 1.5" thick with 50 degree minimum preheat.